5B05 Mechanical Properties of Aluminum
Mechanical properties of aluminum 5B05:
Shear strength τ (MPa): ≥157
Note: The heat does not strengthen the shear resistance of the wire
Heat treatment:
Rapid thermal annealing: heating 350 ~ 410 ℃; vary the effective thickness of the material, holding time 30 ~ 120min; air or water.
Status: rivet aluminum and aluminum alloy wire (HX8 state) [1]
Heat Treatment: rapid thermal annealing: heating 350 ~ 410 ℃; vary the effective thickness of the material, holding time 30 ~ 120min; air or water.
Status: rivet aluminum and aluminum alloy wire (HX8 state)